Haynes 25®
Haynes 25™ has an excellent temperature strength and oxidation resistance to 2000 ®F. Haynes 25™ is hot formable between 1900 ®F- 2300 ®F. Also known as Alloy L605, it is better to cold-work Haynes 25™ for bending, spinning and drawing the components.
Common Trade Names for Haynes 25® include:
- Haynes 25™
Chemical Data for Haynes 25®
- C: .05 -.15
- Mn: 1.0 -2.0
- P: .4
- S: .03
- Si: .4
- Cr: 19.0 -21.0
- Ni: 9.0 -11.0
- Co: BAL
- Co: BAL
- Fe: 3.0
- W: 14.0 -16.0
Available Forms for Haynes 25®
- Wire
- Bar
- Sheet
- Plate
- Tube
- Forgings
- Welding Rod
Trademark Notice: Some names are trade names and/or trademarks of specific manufacturers. Source 1 Alloys is not affiliated with any manufacturer(s). Orders will be filled to meet specifications from all available source(s). Product names are listed solely for reference to help identify products consistent with listed specifications.